<ArticleTitle>Acoustic Emission based Methodology to Evaluate the Fracture Toughness in carbon/epoxy composites</ArticleTitle>
<VernacularTitle>تعیین چقرمگی شکست بین لایه‌ای در چند لایه‌های کامپوزیتی کربن/اپوکسی با روش نشرآوایی</VernacularTitle>
			<FirstPage>379</FirstPage>
			<LastPage>386</LastPage>
			<ELocationID EIdType="pii">668</ELocationID>
			
<ELocationID EIdType="doi">10.22060/mej.2016.668</ELocationID>
			
			<Language>FA</Language>
<AuthorList>
<Author>
					<FirstName>رضا</FirstName>
					<LastName>محمدی</LastName>
<Affiliation>دانشکده مهندسی مکانیک، دانشگاه صنعتی امیرکبیر</Affiliation>

</Author>
<Author>
					<FirstName>میلاد</FirstName>
					<LastName>سعیدی فر</LastName>
<Affiliation>دانشکده مهندسی مکانیک، دانشگاه صنعتی امیرکبیر</Affiliation>
<Identifier Source="ORCID">0000-0003-4950-3007</Identifier>

</Author>
<Author>
					<FirstName>مهدی</FirstName>
					<LastName>احمدی نجف‌ابادی</LastName>
<Affiliation>دانشکده مهندسی مکانیک، دانشگاه صنعتی امیرکبیر</Affiliation>

</Author>
<Author>
					<FirstName>حسین</FirstName>
					<LastName>حسینی تودشکی</LastName>
<Affiliation>دانشکده مهندسی هوافضا، دانشگاه صنعتی امیرکبیر</Affiliation>
<Identifier Source="ORCID">0000-0003-2519-1010</Identifier>

</Author>
</AuthorList>
				<PublicationType>Journal Article</PublicationType>
			<History>
				<PubDate PubStatus="received">
					<Year>2015</Year>
					<Month>07</Month>
					<Day>30</Day>
				</PubDate>
			</History>
		    <Abstract>Fiber-Reinforced Polymer (FRP) composites are an important category of advanced engineering materials. These materials are widely used in the industry due to their unique characteristics such as high specific strength and stiffness. In FRP composite materials, there are several failure mechanisms such as matrix cracking, fiber breakage, fiber/matrix debonding and delamination. Delamination is the most striking one. In this paper, mechanical and acoustic emission (AE) behaviors of delamination are investigated under the actual operation loading modes (i.e. mode I, mode II and the combination of these pure modes). The composite laminates have been fabricated with 14 layers of woven carbon/epoxy prepregs. DCB, ENF and MMB specimens were prepared according to ASTM D5528 and D6671 standards and subjected to the different loading modes. First, inter-laminar fracture toughness of the specimens is calculated using the represented methods in ASTM D5528 and ASTM D6671 standards. Then, fracture toughness of the specimens is determined using the AE-based methods. The results indicate that, the AE-based methods have good applicability to determine the fracture toughness of the composite materials.</Abstract>
			<OtherAbstract Language="FA">کامپوزیت‌ها شاخه مهمی از مواد پیشرفته مهندسی هستند که به دلیل داشتن ویژگی‌های منحصر به فردی به طور گسترده در صنعت از آنها استفاده می‌شود. در این مواد امکان وقوع انواع خرابی‌ها وجود دارد. جدایش بین‌لایه‌ای یکی از شایع‌ترین انواع خرابی‌ در چندلایه‌های کامپوزیتی بوده که در انواع بارگذاری‌های مود I، II یا ترکیبی از این مودها اتفاق می‌افتد. در پژوهش حاضر، به بررسی رفتار مکانیکی و نشرآوایی جدایش بین‌لایه‌ای در کامپوزیت‌های چند لایه کربن/ اپوکسی پرداخته شده و با استفاده از روش نشرآوایی، چقرمگی شکست بین‌لایه‌ای کامپوزیت تعیین می‌شود. نمونه‌های استاندارد، تحت شرایط مختلف بارگذاری مود I، مود II و مود ترکیبی I و II قرار گرفتند. ابتدا، مقادیر چقرمگی شکست بین‌لایه‌ای، با استفاده از روش‌های ارائه شده در استانداردهای ASTM D5528 و ASTM D6671 محاسبه شده‌است. در ادامه، با استفاده از روش نشرآوایی، چقرمگی شکست بین‌لایه‌ای در نمونه‌ها تعیین گردیده‌است. نتایج بدست آمده نشان دهنده تطابق مطلوب مقادیر چقرمگی شکست بدست آمده از روش نشرآوایی با مقادیر حاصل از استاندارد است.</OtherAbstract>
		<ObjectList>
			<Object Type="keyword">
			<Param Name="value">جدایش بین لایه‌ای</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">نشرآوایی</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">چقرمگی شکست بین‌لایه‌ای</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">کربن/اپوکسی</Param>
			</Object>
		</ObjectList>
<ArchiveCopySource DocType="pdf">https://mej.aut.ac.ir/article_668_192fc044e74dffea144f9ac5dc9f3395.pdf</ArchiveCopySource>
</Article>
</ArticleSet>